Ningbo Huayuan Metal Products Co.,Ltd

Manufacturer from China
Verified Supplier
3 Years
Home / Products / Stainless Steel Spring Wire /

302 Grade Bright / Soap-coated Stainless Steel Spring Wire 0.8mm For Various Applications

Contact Now
Ningbo Huayuan Metal Products Co.,Ltd
Visit Website
City:ningbo
Country/Region:china
Contact Person:MrsNelly Zhao
Contact Now

302 Grade Bright / Soap-coated Stainless Steel Spring Wire 0.8mm For Various Applications

Ask Latest Price
Video Channel
Brand Name :TOPONE
Model Number :302
Certification :ISO,SGS,RosH
Place of Origin :China
MOQ :1000kg
Price :Negotiation
Payment Terms :L/C,T/T
Supply Ability :>1000 Tons per month
Delivery Time :10-20 days
Packaging Details :Coil/Spool/Pallet/By customer request
Standard :JIS,EN,ASTM,AISI ,DIN,GB
Surface Treatment :Bright/Soap-coated
Grade :302
Application :Compression/Torsion/Extension Spring
Packing :Coil/Pallet
Diameter :0.8mm
Type :Hard
Tensile Strength :1850-2150N/mm2
more
Contact Now

Add to Cart

Find Similar Videos
View Product Description

Matt 200 / 300 /400 series Stainless Steel Spring Wire

Construction Stainless Steel Spring Wire 302 Stainless Steel Wire JIS G4314 Standard


General Properties

302 is a variations of the 18% chromium / 8% nickel austenitic alloy, which is the most familiar and the most frequently used in the stainless steel family. Alloy 302 is a slightly higher carbon version of 304, often found in strip and wire forms. It is a tough, ductile grade that demonstrates comparable corrosion resistance, is non-magnetic, and is not hardenable by heat treatment. Alloy 302 is usually used in its annealed condition and has a high ease of fabrication and formability.


Chemical Properties:


C Mn Si P S Cr Ni N
302 max: 0.15 max:2.0 max: 0.75 max: 0.045 max: 0.03 min: 17.0 max: 19.0 min: 8.0 max: 10.0 max: 0.10


Mechanical Properties:

Grade Tensile Strength ksi (min) Yield Strength 0.2% ksi (min) Elongation % Hardness (Rockwell B) MAX
302 75 30 40 92


Physical Properties:

Density
lbm/in3
Thermal Conductivity
(BTU/h ft. °F)
Electrical
Resistivity
(in x 10-6)
Modulus of
Elasticity
(psi x 106
Coefficient of
Thermal Expansion
(in/in)/
°F x 10-6
Specific Heat
(BTU/lb/
°F)
Melting
Range
(°F)
at 68°F: 0.285 9.4 at 212°F 72.0 at 70°F 28 9.6 at 32 – 212°F 0.1200 at 32°F to 212°F 2500 to 2590

12.4 at 932 °F

10.2 at 32 – 1000°F





10.4 at 32 – 1500°F


Corrosion Resistance

1, Provides useful resistance to corrosion on a wide range of moderately oxidizing to moderately reducing environments

2, The 18 -19% of chromium which this alloy contains provides resistance to oxidizing environments such as dilute nitric acid.

3, Resistant to moderately aggressive organic acids such as acetic, and reducing acids such as phosphoric.

4,’The 9-11% of nickel contained in this alloy provides resistance to moderately reducing environments.


Machinability

Slow speeds and high feeds will overcome this alloy’s tendency to work-harden

Due to gummy chips, it is recommended that chip breakers are used on all tooling


Weldability

Can best be welded by resistance or shielded fusion methods

Post weld annealing dissolves the chromium carbide and is recommended for maximum resistance to intergranular attack


Hot Working

Uniform heating to 2100oF will allow this allow to be forged, upset and headed successfully

Do not work below 1700oF


Cold Working

Will dramatically increase the hardness of this material; however, it is quite ductile and may readily be drawn, spun and upset

Causes alloy 302 to become magnetic

Post-fabrication annealing is necessary to retain maximum corrosion resistance and a non-magnetic condition


Inquiry Cart 0